Alloy C22 (HASTELLOY C22)

Alias

ASTM B574 N06022
Hastelloy C22
ASME SB574 N06022
2.4602
NiCr21Mo14W

Chemistry

Base Element Ni(Nickel)

Element Min Max
C (Carbon) 0.015%
Co (Cobalt) 2.5%
Cr(Chromium) 20 22.5%
Fe(Iron) 2 6%
Mn(manganese) 0.5%
Mo(Molybdenum) 12.5 14.5%
P(Phosphorus) 0.02%
S(Sulphur) 0.02%
Si(Silicon) 0.08%
V(Vanadium) 0.35%
W(Tungsten) 2.5 4.5%
Ni(Nickel) Bal
Mechanical Property Min Max
Ultimate Tensile Strength (UTS) 690 MPa
0.2% Proof Stress 310 MPa
Elongation 4D 40%

Properties

Corrosion Resistant (HF,H2S04,HCL, HN03)

Disclaimer:
Information is given for illustrative purposes only. Tachart accepts no responsibility for the accuracy of the data contained within or the use of the data by any other party.